Property Temperature Value
Density 23.0 °C Density of 7.8 g/cm³

UNS S17600 Annealed thermal

Property Temperature Value
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.2E-5 1/K
Specific heat capacity 23.0 °C Specific heat capacity of 450 J/(kg·K)

UNS S17600 Annealed electrical

Property Value
Aluminium Aluminium of 0 - 0.4 %
Carbon Carbon of 0 - 0.08 %
Chromium Chromium of 16 - 17.5 %
Iron Iron of 71.3 - 77.6 %
Manganese Manganese of 0 - 1 %
Nickel Nickel of 6 - 7.5 %
Phosphorus Phosphorus of 0 - 0.04 %
Silicon Silicon of 0 - 1 %
Sulfur Sulfur of 0 - 0.03 %
Titanium Titanium of 0.4 - 1.2 %

UNS S17600 Annealed mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 220 GPa -
Elongation 23.0 °C Elongation of 8.6 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Steel
Tensile strength 23.0 °C Tensile strength of 950 MPa -
Yield strength 23.0 °C Yield strength of 590 MPa -

Contact us

Henan Bebon Iron&Steel Co., Ltd.

Xicheng Science & Technology Building High-tech Development Zone, Zhengzhou, China

Tel: +86-371-86151827

E-Mail: [email protected]

PlaceholderContact us

Message