SAE J775 Grade XEV-G
SAE J775 Grade XEV-G general
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | Density of 8.13 g/cm³ |
SAE J775 Grade XEV-G thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 760.0 °C | Coefficient of thermal expansion of 1.53E-5 1/K | The mentioned value is between 20°C and the mentioned temperature |
SAE J775 Grade XEV-G electrical
Property | Value |
---|---|
Aluminium | Aluminium of 1 % |
Carbon | Carbon of 0.1 % |
Chromium | Chromium of 27.8 % |
Iron | Iron of 60.2 - 100 % |
Manganese | Manganese of 8.5 % |
Nickel | Nickel of 0.4 % |
SAE J775 Grade XEV-G mechanical
Property | Temperature | Value |
---|---|---|
Reduction of area | 23.0 °C | Reduction of area of 16 % |
Tensile strength | 23.0 °C | Tensile strength of 1120 MPa |
Yield strength | 23.0 °C | Yield strength of 670 MPa |