SAE J405 Grade XM-17
Equivalent material: AISI XM-17, AISI 216, AISI S21600, SAE 216, SAE S21600, ASTM XM-17, UNS S21600
SAE J405 Grade XM-17 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.9 - 8.2 g/cm³ |
Typical for Austenitic Stainless Steel |
SAE J405 Grade XM-17 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K |
Typical for Austenitic Stainless Steel |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 440 J/(kg·K) |
Typical for Austenitic Stainless Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 21 W/(m·K) |
Typical for Austenitic Stainless Steel |
SAE J405 Grade XM-17 magnetic
Property |
Value |
Carbon |
Carbon of 0.08 % |
Chromium |
Chromium of 17.5 - 22 % |
Manganese |
Manganese of 7.5 - 9 % |
Molybdenum |
Molybdenum of 2 - 3 % |
Nickel |
Nickel of 5 - 7 % |
Nitrogen |
Nitrogen of 0.25 - 0.5 % |
Phosphorus |
Phosphorus of 0.05 % |
Silicon |
Silicon of 0.75 % |
Sulfur |
Sulfur of 0.03 % |
SAE J405 Grade XM-17 electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
SAE J405 Grade XM-17 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 195 GPa |
Typical for Austenitic Stainless Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |