SAE J404 Grade 50B40
Equivalent material: DIN 1.7007, DIN 37CrB1, AISI 50B40H, AISI 50B40, SAE 50B40H, EN 1.7007, ISO 37CrB1E, GB/T A20378, GB/T ML37CrB, UNS H50401, UNS G50401
SAE J404 Grade 50B40 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Chromium Steel |
SAE J404 Grade 50B40 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 9.4E-6 - 1.5E-5 1/K |
Typical for Chromium Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Chromium Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 440 - 494 J/(kg·K) |
Typical for Chromium Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 23 - 50 W/(m·K) |
Typical for Chromium Steel |
SAE J404 Grade 50B40 electrical
Property |
Value |
Boron |
Boron of 1E-3 - 5E-3 % |
Carbon |
Carbon of 0.38 - 0.43 % |
Chromium |
Chromium of 0.4 - 0.6 % |
Iron |
Iron of 97.58 - 98.32 % |
Manganese |
Manganese of 0.75 - 1 % |
Phosphorus |
Phosphorus of 0.04 % |
Silicon |
Silicon of 0.15 - 0.3 % |
Sulfur |
Sulfur of 0.04 % |
SAE J404 Grade 50B40 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Chromium Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Chromium Steel |