JIS G5151 Grade SCPH22

JIS G5151 Grade SCPH22 general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 - 7.9 g/cm³ Typical for Nickel Chromium Molybdenum Steel

JIS G5151 Grade SCPH22 thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K Typical for Nickel Chromium Molybdenum Steel
Melting point - Melting point of 1382 - 1529 °C Typical for Nickel Chromium Molybdenum Steel
Specific heat capacity 23.0 °C Specific heat capacity of 448 - 670 J/(kg·K) Typical for Nickel Chromium Molybdenum Steel
Thermal conductivity 23.0 °C Thermal conductivity of 34 - 54 W/(m·K) Typical for Nickel Chromium Molybdenum Steel

JIS G5151 Grade SCPH22 mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Nickel Chromium Molybdenum Steel
Elongation A5 23.0 °C Elongation A5 of 16 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Nickel Chromium Molybdenum Steel
Reduction of area 23.0 °C Reduction of area of 35 % -
Tensile strength 23.0 °C Tensile strength of 550 MPa -
Yield strength Rp0.2 23.0 °C Yield strength Rp0.2 of 345 MPa -

Contact us

Henan Bebon Iron&Steel Co., Ltd.

Xicheng Science & Technology Building High-tech Development Zone, Zhengzhou, China

Tel: +86-371-86151827

E-Mail: [email protected]

PlaceholderContact us

Message