JIS G5121 Grade SCS14
Equivalent material: AS H6C, DIN GX5CrNiMo19-11-2, EN GX5CrNiMo, NF Z5CND20-10M, NF Z5CND20-8M, NF Z6CND18-12M, BS 316C16, BS 315C16, UNI GX6CrNiMo2011, ÖNORM G-X6CrNiMo1810, EN GX5CrNiMo19-11-2, UNE AM-X7CrNiMo2010, SIS 2343-12, ASTM CF8M, ASTM CPF8M, JIS SCS22, DIN 1.4436, DIN X5CrNiMo17-13-3, DIN X3CrNiMo17-13-3, AFNOR Z7CND18-12-03, BS 316S13, UNI X8CrNiMo1713, SS 2343, SS 2347, AISI 316, SAE 316, JIS SUS316, JIS SUS316TKA, JIS SUS316TF, JIS SUS316FB, JIS SUSF316, JIS SUS316TKC, JIS SUS316TP, JIS SUS316TB, EN X3CrNiMo17-13-3, EN 1.4436, ISO A5, UNS S31600
JIS G5121 Grade SCS14 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.9 - 8.2 g/cm³ |
Typical for Austenitic Stainless Steel |
JIS G5121 Grade SCS14 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K |
Typical for Austenitic Stainless Steel |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 440 J/(kg·K) |
Typical for Austenitic Stainless Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 21 W/(m·K) |
Typical for Austenitic Stainless Steel |
JIS G5121 Grade SCS14 electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
JIS G5121 Grade SCS14 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 195 GPa |
Typical for Austenitic Stainless Steel |
Elongation A5 |
23.0 °C |
Elongation A5 of 28 % |
- |
Hardness, Brinell |
23.0 °C |
Hardness, Brinell of 183 [-] |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |
Tensile strength |
23.0 °C |
Tensile strength of 440 MPa |
- |
Yield strength Rp0.2 |
23.0 °C |
Yield strength Rp0.2 of 185 MPa |
- |