JIS G4901 Grade NCF750 solution treated
JIS G4901 Grade NCF750 solution treated general
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | Density of 8.8 g/cm³ | Typical for Nickel Steel |
JIS G4901 Grade NCF750 solution treated thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | - | Melting point of 1316 - 1595 °C | Typical for Nickel Steel |
Specific heat capacity | 23.0 °C | Specific heat capacity of 456 J/(kg·K) | Typical for Nickel Steel |
Thermal conductivity | 23.0 °C | Thermal conductivity of 10 - 50 W/(m·K) | Typical for Nickel Steel |
JIS G4901 Grade NCF750 solution treated electrical
Property | - | - |
---|---|---|
Processing history |
JIS G4901 Grade NCF750 solution treated mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Nickel Steel |
Hardness, Brinell | 23.0 °C | Hardness, Brinell of 320 [-] | - |
Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Nickel Steel |
Shear modulus | 23.0 °C | Shear modulus of 76 GPa | Typical for Nickel Steel |