Property | Temperature | Value |
---|---|---|
Elongation A5 | 20.0 °C | Elongation A5 of 20 - 25 % |
Reduction of area | 20.0 °C | Reduction of area of 65 % |
Tensile strength | 20.0 °C | Tensile strength of 450 - 680 MPa |
JIS G4315 Grade SUSXM7-WSB mechanical
Property | Value |
---|---|
Carbon | Carbon of 0.08 % |
Chromium | Chromium of 17 - 19 % |
Copper | Copper of 3 - 4 % |
Iron | Iron of 63.34 - 71.5 % |
Manganese | Manganese of 2 % |
Nickel | Nickel of 8.5 - 10.5 % |
Phosphorus | Phosphorus of 0.05 % |
Silicon | Silicon of 1 % |
Sulfur | Sulfur of 0.03 % |