JIS G4107 Grade SNB16
Equivalent material: DIN 40CrMoV47, BS 670-860, ÖNORM 40CrMoV47S, EN 40CrMoV4-6, ASTM B16, ASTM B4D, AISI B16, DIN 1.7711, DIN 40CrMoV4-6, DIN 40CrMoV4-7, AFNOR 40CrMoV4-6, AISI A193B16, SAE A193B16, JIS SNB21-1, JIS SNB21-2, JIS SNB21-3, JIS SNB21-4, JIS SNB21-5, EN 40CrMoV4-7, EN 1.7711, ASTM Grade B16, UNS K14675, UNS K14072
JIS G4107 Grade SNB16 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Chromium Molybdenum Steel |
JIS G4107 Grade SNB16 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.1E-5 - 1.4E-5 1/K |
Typical for Chromium Molybdenum Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Chromium Molybdenum Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 448 - 502 J/(kg·K) |
Typical for Chromium Molybdenum Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 36 - 43 W/(m·K) |
Typical for Chromium Molybdenum Steel |
JIS G4107 Grade SNB16 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Chromium Molybdenum Steel |
Elongation A5 |
23.0 °C |
Elongation A5 of 16 - 18 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Chromium Molybdenum Steel |
Reduction of area |
23.0 °C |
Reduction of area of 50 % |
- |
Tensile strength |
23.0 °C |
Tensile strength of 690 - 860 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 590 - 725 MPa |
- |