JIS G4103 Grade SNCM431

Equivalent material: EN 30CrNiMo8, DIN 30CrNiMo8, NF 30CND8, NF 30NCD8, UNI 30NiCrMo8, DIN 1.6582, DIN 34CrNiMo6, DIN GS-34CrNiMo6, DIN 34CrNiMo6V, DIN 35CrNiMo6, AFNOR 35NCD6, AFNOR 34CrNiMo8, BS 817M40, BS 816M40, BS EN24, UNI 35NiCrMo6(KB), SS 2541, UNE F.127, AISI 4340, SAE 4340, JIS SNCM447, EN 34CrNiMo6, EN 34CrNiMo6V, EN 1.6582, GOST 38Ch2N2MA, ASTM 4337, IS 40Ni2Cr1Mo28

JIS G4103 Grade SNCM431 general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 - 7.9 g/cm³ Typical for Nickel Chromium Molybdenum Steel

JIS G4103 Grade SNCM431 thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K Typical for Nickel Chromium Molybdenum Steel
Melting point - Melting point of 1382 - 1529 °C Typical for Nickel Chromium Molybdenum Steel
Specific heat capacity 23.0 °C Specific heat capacity of 448 - 670 J/(kg·K) Typical for Nickel Chromium Molybdenum Steel
Thermal conductivity 23.0 °C Thermal conductivity of 34 - 54 W/(m·K) Typical for Nickel Chromium Molybdenum Steel

JIS G4103 Grade SNCM431 electrical

Property Value
Carbon Carbon of 0.27 - 0.35 %
Chromium Chromium of 0.6 - 1 %
Iron Iron of 95.04 - 96.63 %
Manganese Manganese of 0.6 - 0.9 %
Molybdenum Molybdenum of 0.15 - 0.3 %
Nickel Nickel of 1.6 - 2 %
Phosphorus Phosphorus of 0.03 %
Silicon Silicon of 0.15 - 0.35 %
Sulfur Sulfur of 0.03 %

JIS G4103 Grade SNCM431 mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Nickel Chromium Molybdenum Steel
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Nickel Chromium Molybdenum Steel

Contact us

Henan Bebon Iron&Steel Co., Ltd.

Xicheng Science & Technology Building High-tech Development Zone, Zhengzhou, China

Tel: +86-371-86151827

E-Mail: [email protected]

PlaceholderContact us

Message