JIS G4052 Grade SCr420H

Equivalent material: DIN 1.7027, DIN 20Cr4, JIS SCr420M, JIS SCr420TK, JIS SCr420HRCH, JIS SCr420RCH, JIS SCr420WCH, JIS SCr22H, JIS SCr420, JIS 20Cr4, EN 20Cr4, EN 1.7027, DIN 1.7028, DIN 20CrS4, EN 20CrS4, EN 1.7028, ISO 20CrS4

JIS G4052 Grade SCr420H general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 - 7.9 g/cm³ Typical for Chromium Steel

JIS G4052 Grade SCr420H thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 9.4E-6 - 1.5E-5 1/K Typical for Chromium Steel
Melting point - Melting point of 1382 - 1529 °C Typical for Chromium Steel
Specific heat capacity 23.0 °C Specific heat capacity of 440 - 494 J/(kg·K) Typical for Chromium Steel
Thermal conductivity 23.0 °C Thermal conductivity of 23 - 50 W/(m·K) Typical for Chromium Steel

JIS G4052 Grade SCr420H electrical

Property Value
Carbon Carbon of 0.17 - 0.23 %
Chromium Chromium of 0.85 - 1.25 %
Iron Iron of 97.21 - 98.28 %
Manganese Manganese of 0.55 - 0.9 %
Phosphorus Phosphorus of 0.03 %
Silicon Silicon of 0.15 - 0.35 %
Sulfur Sulfur of 0.03 %

JIS G4052 Grade SCr420H mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Chromium Steel
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Chromium Steel

Contact us

Henan Bebon Iron&Steel Co., Ltd.

Xicheng Science & Technology Building High-tech Development Zone, Zhengzhou, China

Tel: +86-371-86151827

E-Mail: [email protected]

PlaceholderContact us

Message