JIS G4052 Grade SCM415H
Equivalent material: NF 12CD4FF, UNE 12CrMo4, UNE F.150.J, UNE F.155, JIS SCM415, DIN 1.7262, DIN 15CrMo5, AFNOR 12CD4, SS 2216, JIS SCM415(H), JIS SCM415M, JIS SCM415TK, JIS SCM415RCH, JIS SCM415HRCH, EN 15CrMo5, EN 1.7262
JIS G4052 Grade SCM415H general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Chromium Molybdenum Steel |
JIS G4052 Grade SCM415H thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.1E-5 - 1.4E-5 1/K |
Typical for Chromium Molybdenum Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Chromium Molybdenum Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 448 - 502 J/(kg·K) |
Typical for Chromium Molybdenum Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 36 - 43 W/(m·K) |
Typical for Chromium Molybdenum Steel |
JIS G4052 Grade SCM415H electrical
Property |
Value |
Carbon |
Carbon of 0.12 - 0.18 % |
Chromium |
Chromium of 0.85 - 1.25 % |
Iron |
Iron of 96.91 - 98.18 % |
Manganese |
Manganese of 0.55 - 0.9 % |
Molybdenum |
Molybdenum of 0.15 - 0.35 % |
Phosphorus |
Phosphorus of 0.03 % |
Silicon |
Silicon of 0.15 - 0.35 % |
Sulfur |
Sulfur of 0.03 % |
JIS G4052 Grade SCM415H mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Chromium Molybdenum Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Chromium Molybdenum Steel |