JIS G3561 Grade SWOSC-V
JIS G3561 Grade SWOSC-V general
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | Density of 7.8 - 7.9 g/cm³ | Typical for High Carbon Steel |
JIS G3561 Grade SWOSC-V thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | Coefficient of thermal expansion of 1.32E-5 1/K | Typical for High Carbon Steel |
Max service temperature | - | Max service temperature of 500 °C | Typical for Carbon Steel |
Melting point | - | Melting point of 1289 - 1478 °C | Typical for High Carbon Steel |
Specific heat capacity | 23.0 °C | Specific heat capacity of 486 J/(kg·K) | Typical for High Carbon Steel |
Thermal conductivity | 23.0 °C | Thermal conductivity of 36 W/(m·K) | Typical for High Carbon Steel |
JIS G3561 Grade SWOSC-V electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
JIS G3561 Grade SWOSC-V mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for High Carbon Steel |
Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for High Carbon Steel |
Reduction of area | 23.0 °C | Reduction of area of 40 - 45 % | - |
Shear modulus | 23.0 °C | Shear modulus of 81 GPa | Typical for High Carbon Steel |