JIS G3214 Grade SUSF347H

Equivalent material: ASTM TP347H, ASTM CR347H, ASTM WP347H, ASTM 347H, ASTM F347H, ASTM FP347H, JIS SUS347HTB, JIS SUS347HTP, AISI 347H, SAE 347H, DIN 1.4961, DIN X8CrNiNb16-13, EN X8CrNiNb16-13, EN 1.4961

JIS G3214 Grade SUSF347H general

Property Temperature Value Comment
Density 23.0 °C Density of 7.9 - 8.2 g/cm³ Typical for Austenitic Stainless Steel

JIS G3214 Grade SUSF347H thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K Typical for Austenitic Stainless Steel
Melting point - Melting point of 1230 - 1480 °C Typical for Austenitic Stainless Steel
Specific heat capacity 23.0 °C Specific heat capacity of 440 J/(kg·K) Typical for Austenitic Stainless Steel
Thermal conductivity 23.0 °C Thermal conductivity of 11 - 21 W/(m·K) Typical for Austenitic Stainless Steel

JIS G3214 Grade SUSF347H electrical

Property Temperature Value Comment
Electrical resistivity 23.0 °C Electrical resistivity of 8.5E-7 Ω·m Typical for Austenitic Stainless Steel

JIS G3214 Grade SUSF347H mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 195 GPa Typical for Austenitic Stainless Steel
Elongation A5 23.0 °C Elongation A5 of 29 - 43 % -
Hardness, Brinell 23.0 °C Hardness, Brinell of 187 [-] -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Austenitic Stainless Steel
Reduction of area 23.0 °C Reduction of area of 45 - 50 % -
Shear modulus 23.0 °C Shear modulus of 77 GPa Typical for Austenitic Stainless Steel
Tensile strength 23.0 °C Tensile strength of 480 - 520 MPa -
Yield strength Rp0.2 23.0 °C Yield strength Rp0.2 of 205 MPa -

Contact us

Henan Bebon Iron&Steel Co., Ltd.

Xicheng Science & Technology Building High-tech Development Zone, Zhengzhou, China

Tel: +86-371-86151827

E-Mail: [email protected]

PlaceholderContact us

Message