Property Temperature Value Comment
Density 23.0 °C Density of 8.8 g/cm³ Typical for Nickel Steel

JIS G3127 Grade SL2N255 thermal

Property Temperature Value Comment
Melting point - Melting point of 1316 - 1595 °C Typical for Nickel Steel
Specific heat capacity 23.0 °C Specific heat capacity of 456 J/(kg·K) Typical for Nickel Steel
Thermal conductivity 23.0 °C Thermal conductivity of 10 - 50 W/(m·K) Typical for Nickel Steel

JIS G3127 Grade SL2N255 mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Nickel Steel
Elongation A5 23.0 °C Elongation A5 of 24 - 29 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Nickel Steel
Shear modulus 23.0 °C Shear modulus of 76 GPa Typical for Nickel Steel
Tensile strength 23.0 °C Tensile strength of 450 - 590 MPa -
Yield strength 23.0 °C Yield strength of 255 MPa -

Contact us

Henan Bebon Iron&Steel Co., Ltd.

Xicheng Science & Technology Building High-tech Development Zone, Zhengzhou, China

Tel: +86-371-86151827

E-Mail: [email protected]

PlaceholderContact us

Message