EN 10277-4 Grade 16NiCrS4 treated to ferritic-pearlite structure and turned (+FP+SH)

EN 10277-4 Grade 16NiCrS4 treated to ferritic-pearlite structure and turned (+FP+SH) introduction

As a bright steel product it is used in the form of bars, bright, straight, in various conditions (see DIN EN 10277 : 1999-10).

Equivalent material: DIN 1.5715, DIN 16NiCrS4, EN 1.5715

EN 10277-4 Grade 16NiCrS4 treated to ferritic-pearlite structure and turned (+FP+SH) general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 g/cm³ Typical for Steel

EN 10277-4 Grade 16NiCrS4 treated to ferritic-pearlite structure and turned (+FP+SH) thermal

Property Value
Carbon Carbon of 0.13 - 0.19 %
Chromium Chromium of 0.6 - 1 %
Manganese Manganese of 0.7 - 1 %
Nickel Nickel of 0.8 - 1.1 %
Phosphorus Phosphorus of 0.03 - 0.04 %
Silicon Silicon of 0.4 %
Sulfur Sulfur of 0.02 - 0.04 %

EN 10277-4 Grade 16NiCrS4 treated to ferritic-pearlite structure and turned (+FP+SH) mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 190 - 210 GPa Typical for Steel
Hardness, Brinell 20.0 °C Hardness, Brinell of 156 - 207 [-] -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Steel

Contact us

Henan Bebon Iron&Steel Co., Ltd.

Xicheng Science & Technology Building High-tech Development Zone, Zhengzhou, China

Tel: +86-371-86151827

E-Mail: [email protected]

PlaceholderContact us

Message