Density |
23.0 °C |
Density of 7.8 g/cm³ |
Typical for Steel |
EN 10084 Grade 10NiCr5-4 treated for cold shearing (+S) thermal
Property |
Value |
Carbon |
Carbon of 0.07 - 0.12 % |
Chromium |
Chromium of 0.9 - 1.2 % |
Manganese |
Manganese of 0.6 - 0.9 % |
Nickel |
Nickel of 1.2 - 1.5 % |
Phosphorus |
Phosphorus of 0.04 % |
Silicon |
Silicon of 0.4 % |
Sulfur |
Sulfur of 0.035 % |
EN 10084 Grade 10NiCr5-4 treated for cold shearing (+S) mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 190 - 210 GPa |
Typical for Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Steel |