ASTM A738 Grade B Heat-Treated
ASTM A738 Grade B Heat-Treated general
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Charpy impact energy | Charpy impact energy of 27 J | Heat-Treated | ASTM A738 | Plate |
Tensile strength | Tensile strength of 585 - 705 MPa | Heat-Treated | ASTM A738 | Plate |
Yield strength | Yield strength of 415 MPa | Heat-Treated | ASTM A738 | Plate |
ASTM A738 Grade B Heat-Treated thermal
Property | - | - |
---|---|---|
Supplier Disclaimer |
ASTM A738 Grade B Heat-Treated mechanical
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Carbon | Carbon of 0.2 % | Heat-Treated | ASTM A738 | Plate |
Chromium | Chromium of 0.3 % | Heat-Treated | ASTM A738 | Plate |
Copper | Copper of 0.35 % | Heat-Treated | ASTM A738 | Plate |
Manganese | Manganese of 0.9 - 1.5 % | Heat-Treated | ASTM A738 | Plate |
Molybdenum | Molybdenum of 0.2 % | Heat-Treated | ASTM A738 | Plate |
Nickel | Nickel of 0.6 % | Heat-Treated | ASTM A738 | Plate |
Niobium | Niobium of 0.04 % | Heat-Treated | ASTM A738 | Plate |
Phosphorus | Phosphorus of 0.025 % | Heat-Treated | ASTM A738 | Plate |
Silicon | Silicon of 0.15 - 0.55 % | Heat-Treated | ASTM A738 | Plate |
Sulfur | Sulfur of 0.025 % | Heat-Treated | ASTM A738 | Plate |
Vanadium | Vanadium of 0.07 % | Heat-Treated | ASTM A738 | Plate |