ASTM A710 Grade A, Class 1 As-rolled and precipitation heat treated
ASTM A710 Grade A, Class 1 As-rolled and precipitation heat treated general
Property | Temperature | Value |
---|---|---|
Charpy impact energy | 20.0 °C | Charpy impact energy of 0 - 27 J |
Elongation A50 | 20.0 °C | Elongation A50 of 0 - 20 % |
Tensile strength | 20.0 °C | Tensile strength of 0 - 620 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | Yield Strength Rp0.2, short transverse of 0 - 585 MPa |
ASTM A710 Grade A, Class 1 As-rolled and precipitation heat treated mechanical
Property | Value |
---|---|
Carbon | Carbon of 0 - 0.07 % |
Chromium | Chromium of 0.6 - 0.9 % |
Copper | Copper of 1 - 1.3 % |
Manganese | Manganese of 0.4 - 0.7 % |
Molybdenum | Molybdenum of 0.15 - 0.25 % |
Nickel | Nickel of 0.7 - 1 % |
Niobium | Niobium of 0 - 0.02 % |
Phosphorus | Phosphorus of 0 - 0.03 % |
Silicon | Silicon of 0 - 0.4 % |
Sulfur | Sulfur of 0 - 0.025 % |