ASTM A693 Grade 635 Solution-Treated
Equivalent material: UNS S17600
ASTM A693 Grade 635 Solution-Treated general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 g/cm³ |
Typical for Steel |
ASTM A693 Grade 635 Solution-Treated thermal
Property |
Value |
Aluminium |
Aluminium of 0.4 % |
Carbon |
Carbon of 0.08 % |
Chromium |
Chromium of 16 - 17.5 % |
Manganese |
Manganese of 1 % |
Nickel |
Nickel of 6 - 7.5 % |
Phosphorus |
Phosphorus of 0.04 % |
Silicon |
Silicon of 1 % |
Sulfur |
Sulfur of 0.03 % |
Titanium |
Titanium of 0.4 - 1.2 % |
ASTM A693 Grade 635 Solution-Treated mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 190 - 210 GPa |
Typical for Steel |
Elongation A50 |
23.0 °C |
Elongation A50 of 3 - 5 % |
- |
Hardness, Rockwell C |
23.0 °C |
Hardness, Rockwell C of 32 [-] |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Steel |
Tensile strength |
23.0 °C |
Tensile strength of 825 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 515 MPa |
- |