ASTM A541 Grade 4N Class 1, Quenched and Tempered
ASTM A541 Grade 4N Class 1, Quenched and Tempered general
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | Density of 7.8 g/cm³ | Typical for Steel |
ASTM A541 Grade 4N Class 1, Quenched and Tempered thermal
Property | Value |
---|---|
Carbon | Carbon of 0.23 % |
Chromium | Chromium of 1.25 - 2 % |
Manganese | Manganese of 0.2 - 0.4 % |
Molybdenum | Molybdenum of 0.4 - 0.6 % |
Nickel | Nickel of 2.8 - 3.9 % |
Phosphorus | Phosphorus of 0.03 % |
Silicon | Silicon of 0.3 % |
Sulfur | Sulfur of 0.025 % |
Vanadium | Vanadium of 0.03 % |
ASTM A541 Grade 4N Class 1, Quenched and Tempered mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 23.0 °C | Charpy impact energy of 47 J | - |
Elastic modulus | 23.0 °C | Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | Elongation A50 of 18 % | - |
Poisson's ratio | 23.0 °C | Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | Reduction of area of 48 % | - |
Tensile strength | 23.0 °C | Tensile strength of 725 - 895 MPa | - |