ASTM A541 Grade 1 Quenched and Tempered
ASTM A541 Grade 1 Quenched and Tempered general
Property | Temperature | Value |
---|---|---|
Charpy impact energy | 23.0 °C | Charpy impact energy of 20 J |
Elongation A50 | 23.0 °C | Elongation A50 of 20 % |
Reduction of area | 23.0 °C | Reduction of area of 38 % |
Tensile strength | 23.0 °C | Tensile strength of 485 - 655 MPa |
Yield strength Rp0.2 | 23.0 °C | Yield strength Rp0.2 of 250 MPa |
ASTM A541 Grade 1 Quenched and Tempered mechanical
Property | Value |
---|---|
Carbon | Carbon of 0.35 % |
Chromium | Chromium of 0.25 % |
Manganese | Manganese of 0.4 - 0.9 % |
Molybdenum | Molybdenum of 0.1 % |
Nickel | Nickel of 0.4 % |
Phosphorus | Phosphorus of 0.03 % |
Silicon | Silicon of 0.35 % |
Sulfur | Sulfur of 0.025 % |
Vanadium | Vanadium of 0.05 % |