ASTM A519 Grade 4337
Equivalent material: DIN 1.6582, DIN 34CrNiMo6, DIN GS-34CrNiMo6, DIN 34CrNiMo6V, DIN 35CrNiMo6, AFNOR 35NCD6, AFNOR 34CrNiMo8, BS 817M40, BS 816M40, BS EN24, UNI 35NiCrMo6(KB), SS 2541, UNE F.127, AISI 4340, SAE 4340, JIS SNCM447, JIS SNCM431, EN 34CrNiMo6, EN 34CrNiMo6V, EN 1.6582, GOST 38Ch2N2MA, IS 40Ni2Cr1Mo28
ASTM A519 Grade 4337 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Nickel Chromium Molybdenum Steel |
ASTM A519 Grade 4337 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K |
Typical for Nickel Chromium Molybdenum Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Nickel Chromium Molybdenum Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 448 - 670 J/(kg·K) |
Typical for Nickel Chromium Molybdenum Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 34 - 54 W/(m·K) |
Typical for Nickel Chromium Molybdenum Steel |
ASTM A519 Grade 4337 electrical
Property |
Value |
Carbon |
Carbon of 0.35 - 0.4 % |
Chromium |
Chromium of 0.7 - 0.9 % |
Manganese |
Manganese of 0.6 - 0.8 % |
Molybdenum |
Molybdenum of 0.2 - 0.3 % |
Nickel |
Nickel of 1.65 - 2 % |
Phosphorus |
Phosphorus of 0.04 % |
Silicon |
Silicon of 0.15 - 0.35 % |
Sulfur |
Sulfur of 0.04 % |
ASTM A519 Grade 4337 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Nickel Chromium Molybdenum Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Nickel Chromium Molybdenum Steel |