ASTM A508 Grade 1 Quenched and Tempered
ASTM A508 Grade 1 Quenched and Tempered general
Property | Temperature | Value |
---|---|---|
Elongation A50 | 23.0 °C | Elongation A50 of 20 % |
Reduction of area | 23.0 °C | Reduction of area of 38 % |
Tensile strength | 23.0 °C | Tensile strength of 485 - 655 MPa |
Yield strength Rp0.2 | 23.0 °C | Yield strength Rp0.2 of 250 MPa |
ASTM A508 Grade 1 Quenched and Tempered mechanical
Property | Value |
---|---|
Aluminium | Aluminium of 0.03 % |
Boron | Boron of 3E-3 % |
Calcium | Calcium of 0.02 % |
Carbon | Carbon of 0.35 % |
Chromium | Chromium of 0.25 % |
Copper | Copper of 0.2 % |
Manganese | Manganese of 0.4 - 1.05 % |
Molybdenum | Molybdenum of 0.1 % |
Nickel | Nickel of 0.4 % |
Niobium | Niobium of 0.01 % |
Phosphorus | Phosphorus of 0.03 % |
Silicon | Silicon of 0.4 % |
Sulfur | Sulfur of 0.025 % |
Titanium | Titanium of 0.02 % |
Vanadium | Vanadium of 0.05 % |