ASTM A504 Class C Rim-Quenching Treatment
ASTM A504 Class C Rim-Quenching Treatment general
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | Density of 7.8 g/cm³ | Typical for Steel |
ASTM A504 Class C Rim-Quenching Treatment thermal
Property | Value |
---|---|
Aluminium | Aluminium of 0.06 % |
Carbon | Carbon of 0.67 - 0.77 % |
Chromium | Chromium of 0.25 % |
Copper | Copper of 0.35 % |
Manganese | Manganese of 0.6 - 0.9 % |
Molybdenum | Molybdenum of 0.1 % |
Nickel | Nickel of 0.25 % |
Niobium | Niobium of 0.05 % |
Phosphorus | Phosphorus of 0.03 % |
Silicon | Silicon of 0.15 - 1 % |
Sulfur | Sulfur of 0.005 - 0.04 % |
Titanium | Titanium of 0.03 % |
Vanadium | Vanadium of 0.06 % |
ASTM A504 Class C Rim-Quenching Treatment mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | Elastic modulus of 190 - 210 GPa | Typical for Steel |
Hardness, Brinell | 23.0 °C | Hardness, Brinell of 321 - 363 [-] | - |
Poisson's ratio | 23.0 °C | Poisson's ratio of 0.3 [-] | Typical for Steel |