ASTM A487 Grade 2 Class A, Heat-Treated
ASTM A487 Grade 2 Class A, Heat-Treated general
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | Elongation A50 of 22 % |
Reduction of area | 20.0 °C | Reduction of area of 35 % |
Tensile strength | 20.0 °C | Tensile strength of 585 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | Yield Strength Rp0.2, short transverse of 365 MPa |
ASTM A487 Grade 2 Class A, Heat-Treated mechanical
Property | Value |
---|---|
Carbon | Carbon of 0.3 % |
Chromium | Chromium of 0.35 % |
Copper | Copper of 0.5 % |
Manganese | Manganese of 1 - 1.4 % |
Molybdenum | Molybdenum of 0.1 - 0.3 % |
Nickel | Nickel of 0.5 % |
Phosphorus | Phosphorus of 0.04 % |
Silicon | Silicon of 0.8 % |
Sulfur | Sulfur of 0.035 % |
Tungsten | Tungsten of 0.1 % |
Vanadium | Vanadium of 0.03 % |