ASTM A487 Grade 12 Class B, Heat-Treated general
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | Elongation A50 of 0 - 17 % |
Reduction of area | 20.0 °C | Reduction of area of 0 - 35 % |
Tensile strength | 20.0 °C | Tensile strength of 0 - 725 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | Yield Strength Rp0.2, short transverse of 0 - 585 MPa |
ASTM A487 Grade 12 Class B, Heat-Treated mechanical
Property | Value |
---|---|
Carbon | Carbon of 0.05 - 0.2 % |
Copper | Copper of 0 - 0.5 % |
Manganese | Manganese of 0.4 - 0.7 % |
Molybdenum | Molybdenum of 0.9 - 1.2 % |
Phosphorus | Phosphorus of 0 - 0.04 % |
Silicon | Silicon of 0 - 0.6 % |
Sulfur | Sulfur of 0 - 0.035 % |
Tungsten | Tungsten of 0 - 0.1 % |
Vanadium | Vanadium of 0 - 0.03 % |