ASTM A471 Class 6 Heat-Treated
Equivalent material: ASTM Class 1, ASTM Class 2, ASTM Class 3, ASTM Class 4, ASTM Class 5
ASTM A471 Class 6 Heat-Treated general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 g/cm³ |
Typical for Steel |
ASTM A471 Class 6 Heat-Treated mechanical
Property |
Temperature |
Value |
Comment |
Charpy impact energy |
23.0 °C |
Charpy impact energy of 54 J |
- |
Elastic modulus |
23.0 °C |
Elastic modulus of 190 - 210 GPa |
Typical for Steel |
Elongation A50 |
23.0 °C |
Elongation A50 of 15 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Steel |
Reduction of area |
23.0 °C |
Reduction of area of 43 % |
- |
Tensile strength |
23.0 °C |
Tensile strength of 965 MPa |
- |
Yield strength Rp0.02 |
23.0 °C |
Yield strength Rp0.02 of 860 - 1000 MPa |
- |
Yield strength Rp0.2 |
23.0 °C |