ASTM A409 Grade N08367 Heat-Treated
ASTM A409 Grade N08367 Heat-Treated general
Property | Temperature | Value |
---|---|---|
Tensile strength | 23.0 °C | Tensile strength of 655 - 690 MPa |
Yield strength | 23.0 °C | Yield strength of 310 MPa |
ASTM A409 Grade N08367 Heat-Treated mechanical
Property | Value |
---|---|
Carbon | Carbon of 0.03 % |
Chromium | Chromium of 20 - 22 % |
Manganese | Manganese of 2 % |
Molybdenum | Molybdenum of 6 - 7 % |
Nickel | Nickel of 23.5 - 25.5 % |
Phosphorus | Phosphorus of 0.04 % |
Silicon | Silicon of 1 % |
Sulfur | Sulfur of 0.03 % |