ASTM A403 Grade N08925 Heat-Treated
ASTM A403 Grade N08925 Heat-Treated general
Property | Temperature | Value |
---|---|---|
Elongation A50 | 23.0 °C | Elongation A50 of 20 - 28 % |
Tensile strength | 23.0 °C | Tensile strength of 600 MPa |
Yield strength | 23.0 °C | Yield strength of 295 MPa |
ASTM A403 Grade N08925 Heat-Treated mechanical
Property | Value |
---|---|
Carbon | Carbon of 0.02 % |
Chromium | Chromium of 19 - 21 % |
Manganese | Manganese of 1 % |
Molybdenum | Molybdenum of 6 - 7 % |
Nickel | Nickel of 24 - 26 % |
Nitrogen | Nitrogen of 0.1 - 0.2 % |
Phosphorus | Phosphorus of 0.05 % |
Silicon | Silicon of 0.5 % |
Sulfur | Sulfur of 0.03 % |