ASTM A356 Grade 5 Normalized and Tempered and Stress Relieved

ASTM A356 Grade 5 Normalized and Tempered and Stress Relieved general

Property Temperature Value
Elongation A50 23.0 °C Elongation A50 of 22 %
Reduction of area 23.0 °C Reduction of area of 35 %
Tensile strength 23.0 °C Tensile strength of 485 MPa
Yield strength 23.0 °C Yield strength of 275 MPa

ASTM A356 Grade 5 Normalized and Tempered and Stress Relieved mechanical

Property Value
Carbon Carbon of 0.25 %
Chromium Chromium of 0.4 - 0.7 %
Manganese Manganese of 0.7 %
Molybdenum Molybdenum of 0.4 - 0.6 %
Phosphorus Phosphorus of 0.04 %
Silicon Silicon of 0.6 %
Sulfur Sulfur of 0.03 %