ASTM A333 Grade 4 Heat-Treated
ASTM A333 Grade 4 Heat-Treated general
Property | Temperature | Value |
---|---|---|
Charpy impact energy | 23.0 °C | Charpy impact energy of 18 J |
Elongation A50 | 23.0 °C | Elongation A50 of 16.5 - 30 % |
Tensile strength | 23.0 °C | Tensile strength of 415 MPa |
Yield strength | 23.0 °C | Yield strength of 240 MPa |
ASTM A333 Grade 4 Heat-Treated mechanical
Property | Value |
---|---|
Aluminium | Aluminium of 0.04 - 0.3 % |
Carbon | Carbon of 0.12 % |
Chromium | Chromium of 0.44 - 1.01 % |
Copper | Copper of 0.4 - 0.75 % |
Manganese | Manganese of 0.5 - 1.05 % |
Nickel | Nickel of 0.47 - 0.98 % |
Phosphorus | Phosphorus of 0.03 % |
Silicon | Silicon of 0.08 - 0.37 % |
Sulfur | Sulfur of 0.025 % |