ASTM A304 Grade 8650H
Equivalent material: DIN 1.7228, DIN 50CrMo4, AFNOR 50CrMo4, BS 708M40, BS 50CrMo4, AISI 4150, AISI 4147H, AISI 4150H, AISI 8650H, AISI 4147, AISI 8650, SAE 4150, SAE 4147H, SAE 4150H, SAE 8650H, SAE 4147, SAE 8650, JIS SCM445, JIS SCM445H, EN 50CrMo4, EN 1.7228, ISO 50CrMo4, GOST 50Ch, GB ZG50CrMo, GB C44500, GB ZG50Cr1Mo, ASTM 4150, ASTM 4147, UNS G41500, UNS H41470, UNS H41500, UNS H86500, UNS G41470
ASTM A304 Grade 8650H general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Chromium Molybdenum Steel |
ASTM A304 Grade 8650H thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.1E-5 - 1.4E-5 1/K |
Typical for Chromium Molybdenum Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Chromium Molybdenum Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 448 - 502 J/(kg·K) |
Typical for Chromium Molybdenum Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 36 - 43 W/(m·K) |
Typical for Chromium Molybdenum Steel |
ASTM A304 Grade 8650H electrical
Property |
Value |
Carbon |
Carbon of 0.47 - 0.54 % |
Chromium |
Chromium of 0.35 - 0.65 % |
Copper |
Copper of 0.35 % |
Manganese |
Manganese of 0.7 - 1.05 % |
Molybdenum |
Molybdenum of 0.15 - 0.25 % |
Nickel |
Nickel of 0.35 - 0.75 % |
Phosphorus |
Phosphorus of 0.04 % |
Silicon |
Silicon of 0.15 - 0.35 % |
Sulfur |
Sulfur of 0.04 % |
ASTM A304 Grade 8650H mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Chromium Molybdenum Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Chromium Molybdenum Steel |