ASTM A178 Grade D Heat Treated
ASTM A178 Grade D Heat Treated general
Property | Temperature | Value |
---|---|---|
Elongation A50 | 23.0 °C | Elongation A50 of 30 % |
Tensile strength | 23.0 °C | Tensile strength of 485 MPa |
Yield strength | 23.0 °C | Yield strength of 275 MPa |
ASTM A178 Grade D Heat Treated mechanical
Property | Value |
---|---|
Carbon | Carbon of 0.27 % |
Manganese | Manganese of 1 - 1.5 % |
Phosphorus | Phosphorus of 0.03 % |
Silicon | Silicon of 0.1 % |
Sulfur | Sulfur of 0.015 % |