AISI 1045 Cold Rolled

AISI 1045 Cold Rolled general

Property Temperature Value
Density 23.0 °C Density of 7.8 g/cm³

AISI 1045 Cold Rolled thermal

Property Temperature Value
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.17E-5 1/K
Specific heat capacity 23.0 °C Specific heat capacity of 486 J/(kg·K)
Thermal conductivity 23.0 °C Thermal conductivity of 50.9 W/(m·K)

AISI 1045 Cold Rolled magnetic

Property Value
Carbon Carbon of 0.43 - 0.5 %
Copper Copper of 0.45 %
Iron Balance
Manganese Manganese of 0.6 - 0.9 %
Phosphorus Phosphorus of 0.04 %
Sulfur Sulfur of 0.05 %

AISI 1045 Cold Rolled electrical

Property Temperature Value
Electrical resistivity 23.0 °C Electrical resistivity of 1.62E-7 Ω·m

AISI 1045 Cold Rolled mechanical

Property Temperature Value
Elastic modulus 23.0 °C Elastic modulus of 201 GPa
Tensile strength 23.0 °C Tensile strength of 530 - 685 MPa

Contact us

Henan Bebon Iron&Steel Co., Ltd.

Xicheng Science & Technology Building High-tech Development Zone, Zhengzhou, China

Tel: +86-371-86151827

E-Mail: [email protected]

PlaceholderContact us

Message